Colour that is made, not applied
A painted object gets its colour last. A moulded plastic object gets its colour first, in a compounding plant, weeks or months before anyone sees the finished part. That single difference explains most of what is strange about colour in mass-produced goods: why a kettle body and its lid can drift apart on the shelf, why the same reference number looks paler in a thin wall than in a thick one, why recycled content quietly narrows the palette a designer can realistically ask for. Colour in plastics is a chemistry and process question that happens to end in an aesthetic judgement. The people who specify it well are the ones who understand what happens inside the barrel of an injection moulding machine, and who know which requests are cheap, which are expensive, and which are simply impossible.
The polymer is never a blank page
Designers tend to imagine plastic as a neutral white substrate waiting to receive pigment. It is not. Every base resin arrives with its own optical character — a tint, a level of haze, a translucency — and that character sits underneath everything added to it. Two parts specified to the same colour reference, moulded in two different polymers, will not match unless the colourist compensates for the substrate. That compensation costs pigment, and sometimes it is not achievable at all within the required opacity.
- Polypropylene. Natural PP is a milky, slightly waxy translucent white. It takes clean pastels well but fights deep saturated colours, which need heavy pigment loading to look rich rather than chalky.
- ABS. The workhorse of consumer housings has an ivory to faintly yellow natural state, so cool greys and clean whites need blue toning to stop them reading warm.
- Polycarbonate. Optically clear and excellent for transparent tints, but it carries a faint yellow cast that becomes obvious in large thicknesses and worsens with heat history.
- Polyamide. Nylons yellow noticeably during processing and continue to shift with moisture and age, which is why nylon parts are so often specified black or dark grey.
- Filled compounds. Glass fibre, talc and mineral fillers dull and lighten the base, and glass fibre also produces surface streaking that no colourant can hide.
Pigments, dyes and the masterbatch trade
Two families of colourant do the work. A pigment is an insoluble solid that stays as discrete particles suspended in the polymer, scattering and absorbing light. A dye is a soluble molecule that dissolves into the polymer and colours it the way tea colours water. Pigments give opacity, strength and durability; dyes give transparency and brilliance but tend to be less heat stable and far more prone to migration.
How colourant actually reaches the machine
Very little pigment is added as loose powder. The dominant format is masterbatch: a highly concentrated pigment dispersion carried in a compatible polymer and supplied as pellets, blended with natural resin at the moulding machine at a fixed let-down ratio, typically two to four per cent. The alternative is pre-coloured compound, where the compounder supplies pellets already at final colour, which removes dosing error at the cost of flexibility and minimum order quantities. Liquid colour systems occupy a middle ground and are common in blow moulding. Each route has a different failure mode, and each puts the responsibility for consistency in a different place.
Dispersion: the invisible half of the job
Pigment particles want to stick to each other. Straight from the drum they exist as agglomerates — clusters that must be broken down and wetted by the polymer before the colour develops fully. This happens through shear in the extruder screw, and it is the reason two batches with identical pigment loadings can differ visibly in strength. Under-dispersed pigment shows up as specks, streaks and weak colour, and the same undispersed clusters act as stress concentrators that can reduce impact strength.
- The filter test. Compounders push melt through a fine screen and record the pressure rise; a fast climb signals agglomerates surviving the screw.
- Carbon black is the hardest case. The finest, jettest grades have enormous surface area and are notoriously difficult to disperse, which is why cheap black parts often look brownish or blotchy.
- Screw design matters more than dose. A short, low-shear screw on an old machine can under-develop a masterbatch that performs perfectly elsewhere.
- Blending is not mixing. Tumble-blending pellets ahead of the hopper distributes masterbatch; only melt shear disperses the pigment within it.
The processing window: heat, shear and residence time
A colourant has to survive the process that puts it into the part. Many organic pigments — particularly the bright reds, oranges and yellows that designers reach for — begin to degrade at temperatures that engineering polymers routinely require. A colour approved in polypropylene at 220 degrees Celsius may shift or char in polycarbonate at 300. Residence time compounds the problem: a part moulded in a large machine on a short cycle leaves material sitting hot in the barrel, and the first shots after a pause come out visibly different.
Hot runner systems introduce dead spots where material stagnates and darkens. Regrind — sprues and rejected parts ground and fed back — carries an extra heat history, so a moulder running thirty per cent regrind is effectively running a slightly different, slightly darker colour. Certain pigment chemistries also react with their environment rather than simply degrading: ultramarine blue is attacked by acidic conditions, and some sulphide-based colourants discolour on contact with metals. None of this is visible in a colour chip.
Matching to a physical standard
Colour approval in plastics is done on a moulded plaque, not a printed chip, because thickness, texture and gloss all change the result. A standard workflow has the customer supply a physical master, the colourist produce trial plaques, and a spectrophotometer report the difference numerically alongside a visual assessment in a light booth. Sensible programmes also issue limit standards: a lighter plaque and a darker plaque that bracket what production may ship, so that inspection is a decision rather than an argument.
- Texture changes everything. A gloss surface and a spark-eroded texture moulded from the same pellets can differ by several units of lightness and read as different colours across a parting line.
- Gate and flow lines. Pigment and filler orientation follows the flow front, so long thin parts can show directional shading that only appears at production tool scale.
- Masters drift. Plastic reference plaques age, yellow and scratch; they need controlled storage and periodic replacement against a retained archive.
- Sign off on the real part. Approving a flat plaque and then discovering the curved production part looks different is the single most common cause of late colour disputes.
Opacity, thickness and the geometry trap
Plastic colour travels with thickness in a way that flat materials do not. Unless a part is fully opaque, light passes through, bounces off whatever is behind it and returns changed. A 1.5 mm wall and a 4 mm boss moulded in the same translucent white will not look the same, and a housing with an internal metal shield behind one region will show a shadow. Opacity is bought mainly with titanium dioxide, which is effective, cheap and relentlessly whitening: adding enough of it to hide the internals will lighten and desaturate whatever else is in the recipe.
The hardest colour work in product design is rarely a single part. It is a product with an ABS housing, a polycarbonate lens, a thermoplastic elastomer grip, a painted aluminium trim and a printed label, all specified to the same brand colour and all reaching it by different physics. Matching across materials means accepting that some pairs will never be closer than a visible-but-acceptable difference, and designing the geometry so that those pairs never sit edge to edge in the same plane.
Weathering, migration and the long life of a part
Colour in plastic is a property that ages. Ultraviolet light breaks polymer chains at the surface, and the visible symptoms are fading, chalking and yellowing. Outdoor parts therefore need a stabiliser package — typically a UV absorber plus a hindered amine light stabiliser — and a pigment selection biased towards inorganic chemistries, which are duller but far more lightfast than most organics. Accelerated weathering tests give an early read, but real exposure racks remain the honest test.
- Migration and blooming. Dyes and some low molecular weight additives can travel to the surface over time, leaving a haze or transferring colour to whatever the part touches.
- Contact staining. A soft red overmould pressed against a white housing in a warm warehouse can leave a pink shadow that never comes out.
- Regulatory pressure. Cadmium, lead chromate and other heavy-metal pigments produced brilliant, cheap, heat-stable yellows, oranges and reds; their withdrawal from consumer and food-contact use left substitutes that cost more and tolerate less heat.
- Application rules. Toys, food contact and medical devices each impose their own approved-colourant lists, and a pigment cleared for one is not automatically cleared for another.
Recycled content and the narrowing palette
Post-consumer recycled polymer is the constraint reshaping plastic colour right now. Reclaimed material arrives with a baseline that is grey, beige or muddy green depending on the input stream, and that baseline varies between batches. Bright, clean and pale colours are the first casualties, because covering the substrate demands so much pigment that the recipe becomes expensive and the recycled content becomes pointless. Deep colours and blacks survive best, which is why so much recycled-content product is charcoal.
Sorting technology adds a second constraint. Near-infrared sorters at recycling facilities identify polymers by reflected light, and conventional carbon black absorbs so completely that black parts are invisible to them and end up in the reject stream. Detectable black pigments exist and are being adopted, but they behave differently and cost more. The design response has been partly technical and partly aesthetic: an emerging vocabulary of speckled, heathered and deliberately variable finishes that treats batch variation as a legible sign of recycled content rather than a defect to be hidden.
Specifying colour in plastic without pain
Most colour failures in production trace back to decisions made long before tooling, when a colour was chosen from a printed fan deck by someone with no visibility of the moulding process. A few habits prevent almost all of them.
- Name the polymer before the colour. A colour target is meaningless without the resin, the filler level, the wall thickness and the surface texture attached to it.
- Ask for the moulded plaque early. Approve colour in the actual material at the actual thickness, in the actual finish, and ideally on the actual part.
- Agree a tolerance, not a wish. A numerical limit with matching physical light and dark standards turns an endless subjective debate into a pass or fail.
- Design out cross-material adjacency. Where two different materials must both carry the brand colour, separate them with a shadow gap, a step or a different finish.
- Interrogate the lifetime. Ask what the part will look like after two summers on a windowsill, and specify stabilisation accordingly rather than discovering the answer in warranty claims.
- Treat regrind and recycled content as part of the recipe. Fix the percentage and hold it, because a moulder who quietly raises it will darken the colour.
Plastic rewards designers who accept its terms. Colour that is compounded into the material rather than laid on top of it does not chip, scratch through to a different shade, or need a second production process. That is a genuine advantage, and it is available to anyone willing to specify with the barrel temperature in mind.